Tempered Glass
4-5× stronger than annealed glass with safe fragmentation
Thickness: 3.8mm – 19mmMax Panel Size: 3,300mm × 15,000mmStrength: 4-5× ordinary glass
Ver Detalles
Insulated Glass
Superior thermal and acoustic insulation for energy-efficient buildings
Spacer Options: 6mm, 9mm, 12mm, 15mm, 20mmGlass Options: Clear, Low-E, tinted, reflectiveGas Fill: Air or Argon (automated filling line)
Ver Detalles
Laminated Glass
Impact-resistant safety glass with superior sound and UV blocking
Configuration: 2-layer, multi-layer, or jumbo laminatedInterlayer: PVB (standard) or SGP (structural)UV Blocking: > 99% ultraviolet radiation
Ver Detalles
Enameled Glass
Decorative ceramic frit glass with permanent color and pattern
Colors: Custom RAL / Pantone color matchingPatterns: Dots, lines, gradients, custom designsDurability: Will not fade, peel, or delaminate
Ver Detalles
Low-E Glass
Energy-efficient coating that reflects heat while letting light through
Coating Type: Soft-coat (sputtered) or Hard-coat (pyrolytic)Emissivity: 0.05 - 0.15 (vs 0.84 for uncoated glass)Visible Light Transmission: 60% - 80%
Ver Detalles
Curved Tempered Glass
Hot-bent and cold-bent architectural glass from a 500 mm minimum radius
Thickness Range: 6mm, 8mm, 10mm, 12mm, 15mm, 19mmMinimum Radius: 500mm (6mm panels)Max Panel Size: 3,300mm × 15,000mm